Abstract
1 min read
The combination (AIM-ME) of atomic layer deposition in metal–organic frameworks (MOFs) and metal exchange (ME) is introduced as a technique to install dispersed metal atoms into the mesoporous MOF, NU-1000. Zn-AIM, which contains four Zn atoms per Zr6 node, has been synthesized through AIM and further characterized through density functional calculations to provide insight into the possible structure. Zn-AIM was then subjected to modification via transmetalation to yield uniform porous materials that present nonstructural Cu, Co, or Ni atoms.
Leighanne C. Gallington, In S. Kim, Wei-Guang Liu, Andrey A. Yakovenko, Ana E. Platero‐Prats, Zhanyong Li, Timothy C. Wang, Joseph T. Hupp, Omar K. Farha, Donald G Truhlar, Alex B. F. Martinson, Karena W. Chapman
Jian Liu, Jingyun Ye, Zhanyong Li, Ken‐ichi Otake, Yijun Liao, Aaron W. Peters, Hyunho Noh, Donald G Truhlar, Laura Gagliardi, Christopher J. Cramer, Omar K. Farha, Joseph T. Hupp
Ana E. Platero‐Prats, Aaron B. League, Varinia Bernales, Jingyun Ye, Leighanne C. Gallington, Aleksei Vjunov, Neil M. Schweitzer, Zhanyong Li, Jian Zheng, B. Layla Mehdi, Andrew Stevens, Alice Dohnálková, Mahalingam Balasubramanian, Omar K. Farha, Joseph T. Hupp, Nigel D. Browning, John L. Fulton, Donald M. Camaioni, Johannes A. Lercher, Donald G Truhlar, Laura Gagliardi, Christopher J. Cramer,
Discussion(0)
No comments yet. Be the first to comment.