Solid solutions of the formula La2−xLnxCuO4 (Ln = Pr, Nd) possess the orthorhombic structure of La2CuO4 for small values of x and transform to the tetragonal Nd2CuO4 structure at a critical value of x. At the critical composition, there is an abrupt change in specific volume as well as the
c
a
ratio. The material exhibits temperature-independent electrical resistivity below the critical value x and semiconducting behaviour above it. The specific volume and
c
a
ratio smoothly decrease with increase in x in the La2Cu1−xNixO4 system, although the solid solution possess the tetragonal K2NiF4 structure when x>0.1. Compositions with x>0.1 exhibit a gradual semiconductor metal transition similar to that of La2NiO4, the transition temperature decreasing with increasing x.