Secondary Passive Film Failure Induced by Chloride for Laser Directed Energy Deposition Nickel-Based Superalloys During Electrochemical Machining — Pengfei Guo (2022) | RDL Network
Back
Cite
Save
Save for later
Share
Home
Publications
Secondary Passive Film Failure Induced by Chloride for Laser Directed Energy Deposition Nickel-Based Superalloys During Electrochemical Machining
Shared by
Digby D Macdonald
University of California, Berkeley
Secondary Passive Film Failure Induced by Chloride for Laser Directed Energy Deposition Nickel-Based Superalloys During Electrochemical Machining
Article
2022
en
Authors
+6 more
PG
Pengfei Guo
XL
Xin Lin
Digby D Macdonald
University of California, Berkeley
Discussion
(0)
Sign in
to like and join the discussion.
No comments yet. Be the first to comment.
Related publications
Article
2022
Secondary Passive Film Failure Induced by Chloride for Laser Directed Energy Deposition Nickel-Based Superalloys During Electrochemical Machining
Pengfei Guo
,
Xin Lin
,
Digby D Macdonald
,
Inger Odnevall
,
Shaoli Zhang
,
Yufeng Zhang
,
Jianrui Liu
,
Hongbo Lan
,
Weidong Huang
Article
2023
Chloride Induced Secondary Passive Film Failure for Laser Additive Manufacturing Nickel-Based Superalloys during Electrochemical Machining
Pengfei Guo
,
Xin Lin
,
Digby D Macdonald
,
Inger Odnevall
,
Shaoli Zhang
,
Yufeng Zhang
,
Changjian Lin
,
Qiang Wu
,
Yuan Yang
,
Weidong Huang
Article
1988
Breakdown of the Passive Film on Polycrystal and Single Crystal (100) Nickel by Chloride
Kuan‐Shaur Lei
,
Digby D Macdonald
,
Bruce G. Pound
,
B. E. Wilde
Article
2007
Electrochemical Properties of Nonstoichiometric LiNi0.5Mn1.5O4− Thin-Film Electrodes Prepared by Pulsed Laser Deposition
Huarong Xia
,
Yuebo Meng
,
Li Lü
,
Gerbrand Ceder
Article
1988
ChemInform Abstract: Breakdown of the Passive Film on Polycrystal and Single‐Crystal (100) Nickel by Chloride
Kuan Lei
,
Digby D Macdonald
,
Bruce G. Pound
,
B. E. Wilde
Discussion(0)