Skip to content
RDL
Network
Ecosystem
Switch app
TR
About
FAQ
Sign in
Get started
On the Shape of Stress Corrosion Cracks in Water-Cooled Nuclear Power Reactor Piping — Daniel P. Kramer (2012) | RDL Network
Back
Cite
Save
Save for later
Share
Home
Publications
On the Shape of Stress Corrosion Cracks in Water-Cooled Nuclear Power Reactor Piping
Shared by
Digby D Macdonald
University of California, Berkeley
On the Shape of Stress Corrosion Cracks in Water-Cooled Nuclear Power Reactor Piping
Article
2012
en
Authors
DK
Daniel P. Kramer
SL
Sang‐Kwon Lee
Digby D Macdonald
University of California, Berkeley
Abstract
1 min read
Abstract not Available.
Discussion
(0)
Sign in
to like and join the discussion.
No comments yet. Be the first to comment.
Related publications
Article
2013
On the Shape of Stress Corrosion Cracks in Water-Cooled Nuclear Power Reactor Piping
Sang‐Kwon Lee
,
Daniel P. Kramer
,
Digby D Macdonald
Article
2014
On the shape of stress corrosion cracks in sensitized Type 304 SS in Boiling Water Reactor primary coolant piping at 288 °C
Sang‐Kwon Lee
,
Daniel P. Kramer
,
Digby D Macdonald
Chapter in a book
2012
Electrochemical techniques for monitoring and controlling corrosion in water-cooled nuclear reactor systems
Digby D Macdonald
Article
1980
Measurement of pH in Simulated Water-Cooled Nuclear Reactor Heat Transport Circuits
Digby D Macdonald
,
Paul R. Wentrcek
,
Arthur C. Scott
Chapter in a book
1981
3 3. Electrochemical thermodynamics of water-cooled nuclear reactor heat-transport circuits
Digby D Macdonald
Discussion(0)
No comments yet. Be the first to comment.