DD98M alloy is a second generation nickel-based single crystal superalloy without Re addition, which is developed by Institute of Metal Research, Chinese Academy of Sciences. It is a combination of attractively strong points including high strength and low cost. In this work, Ni-based single crystal superalloy DD98M was adopted as the substrate material. Two types MCrAlY (M denote metal) coatings were deposited on DD98M specimen by arc ion plating and YSZ topcoat (TC) were deposited on the substrate by electron beam physical vapor deposition (EB-PVD) on the NiCrAlY bond coat (BC). Experimental results showed that the application of the NiCrAlY and NiCoCrAlYHfSi coatings improved the oxidation resistance of DD98M obviously at 1000 °C. The adhesion of oxide scale of NiCoCrAlYHfSi coating was much better than that of NiCrAlY coating. TBCs application greatly enhanced the operating temperature and significantly improved the durability of the substrate. The thermal growth oxidation (TGO) between the bond coat and topcoat play an important role in adhesion of the whole coating system.
Alexandros Kakaroglou, Gill Scheltjens, Bernard Nisol, Iris De Graeve, Guy Van Assche, Bruno Van Mele, Rudolph Willem, Monique Biesemans, François Reniers, Herman Terryn
Discussion(0)
No comments yet. Be the first to comment.