Discussion on 'Stochastic modeling of pitting corrosion: a new model for initiation and growth of multiple pits' — Robert Melchers (2008) | RDL Network
Back
Cite
Save
Save for later
Share
Home
Publications
Discussion on 'Stochastic modeling of pitting corrosion: a new model for initiation and growth of multiple pits'
Shared by
Robert Melchers
Newcastle University
Discussion on 'Stochastic modeling of pitting corrosion: a new model for initiation and growth of multiple pits'
Article
2008
en
Authors
Robert Melchers
The University Of Newcastle
Discussion
(0)
Sign in
to like and join the discussion.
No comments yet. Be the first to comment.
Related publications
Article
2008
Discussion on “Stochastic modeling of pitting corrosion: A new model for initiation and growth of multiple pits” by A. Valor, F. Caleyo, L. Alfonso, D. Rivas, J.M. Hallen [Corros. Sci. 49 (2007) 559]
Robert Melchers
Corrosion Science
Article
1985
Solute‐Vacancy Interaction Model and the Effect of Minor Alloying Elements on the Initiation of Pitting Corrosion
Mirna Urquidi
,
Digby D Macdonald
Article
2019
Studies on Pitting Corrosion of Al-Cu-Li Alloys Part II: Breakdown Potential and Pit Initiation
Elmira Ghanbari
,
Alireza Saatchi
,
Xiaowei Lei
,
Digby D Macdonald
Article
2020
Monte-Carlo Simulation of Pitting Corrosion with a Deterministic Model for Repassivation
George R. Engelhardt
,
Digby D Macdonald
Article
2006
Copper composition influence on pitting and intergranular corrosion of model AlMgSi alloys
Hong Zhan
,
K. Heylen
,
Iris De Graeve
,
Herman Terryn
,
J.H.W. de Wit