Atomic layer deposition of crystalline epitaxial MoS<sub>2</sub> nanowall networks exhibiting superior performance in thin-film rechargeable Na-ion batteries — M. B. Sreedhara (2018) | RDL Network
Atomic layer deposition of crystalline epitaxial MoS<sub>2</sub> nanowall networks exhibiting superior performance in thin-film rechargeable Na-ion batteries
Journal of Materials Chemistry A 6(5): 2302-2310
Article 2018 English
Authors
MS
M. B. Sreedhara
SG
Subhra Gope
BV
Badri Vishal
Abstract
1 min read
Nanowall network of MoS<sub>2</sub> grown by atomic layer deposition shows single crystalline nature and epitaxial relationship with <italic>c</italic>-sapphire. The nanowall network grown directly on current collector exhibits high capacity, remarkable stability, cyclability and high rate capability over a wide range of operating currents.